Quote:
Originally Posted by BonelessSugar
Cleaned it up. The melty temperature was a lot easier to figure out this time. It's just not sticking how I want it to. Might need to buy actual flux, might not be the right aluminum, could be the oxide layer you were talking about, or might just have the wrong sticks. It's strong enough with one layer of like 6 (inner bottom, inner both sides, outer top, outer both sides). Can't break it with pliers, but didn't flow into the joint no matter how much I tried to persuade it. It's PROBABLY strong enough, but I'm just gunna order some flux for $15 and snap it in my vice with a long metal pipe and try again next week. If it doesn't work I'll delegate it to the passages pegs that I don't use or just toss it.
|
why not just buy one off ebay and save your self a lot of headache
|
|
|